흡습제식 공기 건조기의 작동 원리: 타워 내부에서 실제로 일어나는 일

Water in a compressed air line can corrode piping, freeze in exposed valves, or disrupt a paint finish. A compressor takes in ambient air containing water vapor. Compression increases the vapor’s partial pressure, and as the discharged air cools below its pressure dew point, some of that vapor condenses. An aftercooler, separator, and drain remove bulk liquid upstream. The desiccant dryer removes the vapor that remains, reducing the risk of condensation farther downstream.

This article covers adsorption dryers for compressed air systems: the twin-tower units you see next to compressors in plants, and the small single-cartridge canisters on garage and workshop setups. It does not cover the hopper dryers that plastic processors use to dry resin pellets, or the rotary desiccant wheels used in building HVAC. Same word, different machines.

산업용 설비실에 있는 스크류식 공기 압축기 옆에 설치된 트윈 타워형 흡습제식 공기 건조기. 이 작동 원리 안내서에서 설명하는 표준 기종입니다.
A twin tower desiccant dryer plumbed beside its compressor, the hardware behind the working principle described below.

The desiccant air dryer working principle comes down to adsorption. Compressed air passes through a packed bed, and water molecules accumulate on the internal surfaces of the porous material. A regenerative dryer restores part of the bed’s capacity by lowering the water-vapor partial pressure, heating the bed, or combining those methods. The regeneration stream then carries away the released moisture.

Adsorption and absorption

흡착

Water accumulates on the internal surfaces of a porous solid. A suitable dry purge stream, with heat where required, releases and carries away the adsorbed water.

흡수

Water enters the bulk of another material. A deliquescent drying salt, for example, takes up water and forms a liquid solution.

Most industrial regenerative dryers use two towers. While Tower A dries the process air, Tower B is isolated and regenerated. A conventional heatless dryer depressurizes the offline tower and sends dry purge air through it. Heated designs may include a separate cooling stage. The regenerated tower returns to near line pressure before switching to limit disturbance to the downstream air supply. The controller can switch on a timer or, where supported, use a dew point signal to adjust the drying interval. [1, 3]

Smaller setups often use a single canister of indicating silica gel. A color change gives a visual indication of moisture uptake. When the cartridge reaches its service limit, replace it or reactivate it according to the supplier’s instructions. For intermittent workshop tools or a point-of-use paint line, a cartridge can be practical when flow and outlet quality are within its rating.

The twin-tower cycle, four moves

1

Tower A adsorbs moisture while Tower B depressurizes

2

Tower B releases moisture into the regeneration stream

3

Tower B re-pressurizes to line pressure

4

Valves switch roles, Tower A regenerates while Tower B dries

That is the machine. The cycle tells you how the towers take turns, but it tells you nothing about what the towers are filled with. The fill is where the real differences live, and it decides how dry your air can actually get.

What Is Actually in the Beds: The Three Drying Materials

Open a twin-tower dryer and you will find one of three families of material, or a deliberate combination of them. The choice is not cosmetic. It sets the floor under your dew point, decides how the bed reacts to oil and liquid water, and determines what you will pay for on replacement day.

작업대 위에서 반투명한 실리카겔 구슬, 흰색 활성 알루미나 구슬, 회색 분자 체 펠릿 등 세 가지 흡습제 충전재를 나란히 비교한 모습
Three commonly used drying media: silica gel beads, activated alumina spheres, and molecular sieve pellets.

Silica gel: moisture uptake and indicating grades

Silica gel is often sold as translucent beads. Some grades contain a moisture indicator, and the color change depends on the formulation. Silica gel can hold substantial moisture at higher relative humidity and is used in some point-of-use and regenerative dryers. In the low water-vapor conditions near the outlet of a deep-drying bed, molecular sieves can retain more water than conventional silica gel. Check the grade’s water-uptake data and its resistance to attrition under the intended operating conditions.

Activated alumina: a common fill for −40 °C PDP designs

Activated alumina is a common fill in industrial twin-tower beds. It can handle much of the incoming water-vapor load in suitably rated dryers, including many systems designed for a −40 °C pressure dew point. Formed alumina grades are available in several bead sizes. Compare crush strength at the same size and test method, and use the declared temperature and relative humidity when comparing static water uptake. The dryer still needs upstream separation and drainage to protect the bed from bulk liquid.

Molecular sieves: deep drying at low vapor pressure

The molecular sieves used in these dryers are typically synthetic zeolites, crystalline aluminosilicates with well-defined pore structures. Type 4A has a nominal opening of about 4 Å. The nominal designation of 13X describes a commercial grade, and pore access depends on the window connecting its larger cages. These materials can retain water at low vapor partial pressures, which makes them useful in some systems specified for −70 °C pressure dew point. The rated result depends on the bed, cycle, and inlet conditions. Type 13X can also adsorb carbon dioxide, but a static CO₂ capacity does not establish a dryer’s CO₂ removal performance under humid feed conditions. A replacement grade should be checked for regeneration compatibility and protected from oil carryover.

Layered beds: bulk vapor removal and final drying

A layered bed can use activated alumina at the process-air inlet to remove much of the water-vapor load, then a downstream molecular sieve layer for final drying. The physical position of each layer depends on the flow direction. A properly designed upstream separator and filtration train protects the fill from liquid water and oil aerosols. Select the layer sequence and quantity with the dryer manufacturer.

Inside a layered bed

Low-PDP dry air out

Molecular sieve layer, downstream

Removes traces of water vapor

Activated alumina layer, upstream

Removes much of the incoming water vapor

Wet compressed air in

Example of an upflow drying bed. Follow the specified loading order for your dryer.

Drying materials compared

재료 Deep drying role Water uptake Protection required 기계적 특성 Typical application
실리카겔 Depends on grade and cycle Substantial at higher humidity Protect from liquid and oil Grade-specific Point-of-use cartridges and regenerative dryers
활성 알루미나 Common in −40 °C PDP designs Handles bulk vapor load Protect from liquid and oil Specify strength and attrition by size Industrial twin-tower beds
분자체 4A Can support deep drying in rated systems Retains water at low vapor pressure Protect from liquid and oil Grade-specific Deep-drying or polishing layers
분자체 13X Can support deep drying in rated systems Adsorbs water and can also adsorb CO₂ Protect from liquid and oil Grade-specific Specialty duties when grade is specified
Layered bed Downstream layer polishes the air Upstream layer handles bulk vapor Requires upstream pretreatment Depends on each layer Dryers designed for staged moisture removal

Check the performance of the complete dryer before choosing a material. Silica gel, alumina and molecular sieves each have grade-specific uptake characteristics. A −40 °C or −70 °C pressure dew point is a system rating that depends on the inlet air, media, bed design and regeneration cycle. Liquid water and oil carryover can impair any of these fills. When changing the media, confirm that the existing purge, heating and cooling stages suit the new grade.

Regeneration restores the working capacity the next drying cycle needs, and its energy cost shows up on the compressed air bill.

How the Beds Come Back: Regeneration and Its Real Cost

Water loading on the desiccant depends on water-vapor partial pressure and bed temperature. A dry purge lowers the vapor partial pressure around the adsorbent. Heating lowers the amount of water the bed retains at a given vapor pressure, while the regeneration stream carries the released moisture out. Four common approaches use these effects in different ways.

공장 설비실에서 오프라인 타워가 재생되는 동안 트윈 타워 흡습식 공기 건조기의 머플러에서 습한 퍼지 공기가 배출되는 모습
Regeneration in action: humid purge air leaving the muffler while the offline tower gives up its moisture.

Heatless regeneration expands a portion of the dried product air and passes it through the idle bed, usually near atmospheric pressure. It requires no regeneration heater or blower. Natural Resources Canada gives 15–20% of rated dryer capacity as a typical purge demand for an uncontrolled heatless design. For example, a dryer rated for 1,000 scfm that uses 150 scfm for purge delivers about 850 scfm before other cycle losses. Check the rated and average purge flow for the unit and use the same reference conditions when comparing flow figures. [2]

Internally or externally heated dryers warm the regeneration stream and can reduce demand for compressed purge air. A heated blower purge dryer typically uses ambient air for the heating stage. Some models use dry compressed air for cooling or repressurization, so compare consumption across the full cycle. Include heater and blower power, maintenance, and compressor power for any compressed air the dryer uses. [1, 3]

Heat-of-compression dryers use hot compressor discharge air to regenerate the bed. The design must be compatible with the compressor arrangement and have enough discharge heat over the expected operating range. Outlet dew point and use of auxiliary heat or purge depend on the unit and load. Ask for performance data at the loads your plant actually runs. [1]

An upstream refrigerated dryer can reduce the moisture load on a downstream adsorption dryer. Before adding one to an existing heatless installation, check the manufacturer’s rated inlet temperature and flow range, as well as whether the control and purge settings suit the combined system. Inlet temperature affects adsorption and the amount of vapor in saturated inlet air. Use the dryer’s operating limits when assessing cold inlet conditions. [3]

Regeneration methods and their true cost

방법 Compressed air consumed Main energy inputs Equipment considerations PDP selection
Heatless Typically 15–20% of rated capacity for uncontrolled units Compressor energy for purge and cycle losses No regeneration heater or blower Confirm the complete dryer rating
Heated (internal/external) Typically less than heatless designs Heater power and compressed air Heating and cooling sequence Confirm the complete dryer rating
Heated blower purge Design-dependent, including cooling air Heater, blower and any compressed air Ambient conditions affect design and selection Confirm the complete dryer rating
Heat of compression Design-dependent Discharge heat plus any auxiliary power Needs compatible compressor and duty Verify over the expected load range

If the regeneration stage is too short or the purge supply is inadequate, retained moisture can accumulate and outlet dew point can rise over successive cycles. A brief excursion near switchover can reflect valve timing, repressurization, residual bed heat, or the sampling setup. Compare the two towers across several cycles and judge excursions against the downstream specification.

The regeneration scheme sets what the machine costs to run. Which dew point you actually need decides whether you should be paying it at all.

A regeneration review starts with the dryer model, actual purge flow, outlet dew point trend, and the approved fill. Share those details with Jalon to discuss grade compatibility.

Review My Regeneration Setup

Do You Actually Need One: Dew Point Classes and the Fork

Pressure dew point (PDP) is the temperature at which the compressed air reaches water-vapor saturation at a stated pressure. ISO 8573-1 gives PDP limits for water Classes 1–5, from ≤ +7 °C for Class 5 to ≤ −70 °C for Class 1. The standard also defines other water classes and specifies particles and oil separately. Compare readings on the same pressure basis, because an atmospheric-pressure sample has a different dew point than the same air at line pressure. [4]

Refrigerated dryers chill the air and drain the condensate. A properly rated refrigerated unit can meet a +3 °C pressure dew point and may be sufficient for shop tools or processes in temperature-controlled buildings. Adsorption dryers are used where the line is exposed to freezing conditions or equipment needs a lower PDP. Paint and powder coating, laser cutting, instrument air, and food or pharmaceutical processing can all have application-specific requirements. Check the point-of-use specification and lowest line temperature before assigning any of these applications a water class.

압축 공기실에 스테인리스강 배관을 통해 직렬로 연결된 냉동식 건조기와 트윈 타워 흡습식 공기 건조기
In a combined system, refrigeration reduces the vapor load before the adsorption stage.

Refrigerated and adsorption dryers can also be used in series when the units are designed to work together. The refrigerated stage removes part of the water-vapor load by cooling and draining condensate, and the adsorption stage lowers the remaining moisture content. During startup, verify that outlet PDP has stabilized within specification before admitting air to a moisture-sensitive process. The time required depends on the equipment and bed condition.

Dew point class to technology mapping

ISO 8573-1 water class Maximum pressure dew point Common dryer option Illustrative applications
Class 4 / Class 5 ≤ +3 °C / ≤ +7 °C 냉각식 건조기 General shop air and above-freezing lines
Class 3 ≤ −20 °C Rated adsorption dryer Selected process air and outdoor services
Class 2 ≤ −40 °C Rated adsorption dryer Some instrument air and coating systems
Class 1 ≤ −70 °C Adsorption dryer specifically rated for this duty Selected moisture-sensitive processes

One discipline turns this from a quiz into a decision. Air is not “dry” in general; it is dry to a class, and the class belongs in your purchase order, not in a verbal description. And the fork has a waste side too. Buying a twin-tower desiccant dryer for a shop that only ever needed +3°C class air means paying purge losses and maintenance for capability you will never use.

Once the class is on paper, the next buying decision is the fill itself, and that is where a purchase order earns its keep.

Specifying the Fill: Buying Desiccant by Parameters, Not by Liters

A replacement bed is bought by the liter or the kilogram, but two fills of the same volume can behave completely differently. The difference is in the datasheet, and every parameter on it maps to a failure mode you have either planned for or not.

The five parameters that decide bed behavior

Static water adsorption, reported as a mass percentage, shows how much water a sample holds at equilibrium under the stated conditions. Request the test temperature, relative humidity, sample preparation, and reporting basis. Comparing an alumina value measured at 60% RH with a sieve value measured at 75% RH cannot establish which material performs better in the same dryer. Ask for dynamic working capacity or outlet dew point data under a representative cycle when evaluating a change of grade.

Crush strength, often reported in newtons per bead, describes resistance to a specified compressive load. A larger particle can show a higher force at failure simply because of its geometry. For acceptance, compare the same size range, particle form and test method, and agree on whether the supplier reports a minimum or an average. Track fines separately through an attrition test.

Attrition is mechanical wear that can generate fines during handling and service. Dust can collect in afterfilters, valves, or exhaust mufflers and may increase pressure drop. Request the method and sampling basis behind any reported mass percentage, and distinguish wear generated during the test from loose dust already present in the shipment.

Bulk density in grams per milliliter converts a defined tower fill volume to an estimated media mass. Loose-poured and tapped density can differ. Use the density basis that matches the loading procedure, and compare quotes against the mass required for the approved tower fill, including any agreed allowance for handling and settlement.

Size and regeneration match close the list. Bead diameters from 1.6-2.5 mm to 3-5 mm (and 1/16″ or 1/8″ pellet forms) set the pressure drop across the bed. Each material also releases its water at different temperatures, so the fill has to tolerate the regeneration scheme you actually run.

Fill parameters mapped to failure modes

매개변수 What it tells you Failure mode if ignored Acceptance action
Static water adsorption (mass %, with conditions) Equilibrium water uptake Misleading comparisons across test conditions Compare at identical RH and temperature. Verify dynamic performance separately.
Crush strength (N) Survival of loading and cycling Fines generation, dust downstream Sample and crush against contract value
Attrition (mass %) Fines generated in a defined wear test Potential dust accumulation or filter loading Specify the test method and lot acceptance limit
Bulk density (g/ml) Kilograms per tower volume Hidden cost per tower Convert quotes to cost per tower, not per liter
Size and regeneration match Pressure drop and regeneration fit Bed fails to regenerate fully Match material grade to your regeneration temperature

The acceptance routine that protects the purchase

Require a certificate of analysis for each batch and confirm that the supplier can trace the lot and provide retained samples if agreed. On arrival, sample the lot and compare it with the contract values. Confirm the package weight, moisture barrier, storage requirements and handling method before ordering. Drums, cartons, and bulk bags suit different changeout arrangements. Choose a format that allows the crew to maintain lot traceability and keep unopened fill dry.

Fill purchase checklist

  • Dew point class and oil exposure written on the PO.
  • Material and layering chosen against the matrix above.
  • Parameters with test conditions in the contract.
  • Batch COA and retained-sample traceability required.
  • Packaging and changeout plan agreed.

The matrix below is the whole decision in one view.

Fill choice matrix with boundaries

Fill plan Fits when Boundary: when it stops working
활성 알루미나 The dryer is rated for the duty with the specified alumina grade Check the inlet conditions and cycle before substituting another grade
분자체 The specified grade is approved for the dryer and deep-drying target Check purge or heating conditions and upstream contamination controls
Layered alumina + sieve Separate bulk drying and final polishing are part of the design Match each layer to the specified loading, flow direction and regeneration cycle
Air-dryer-grade alumina The dryer specification calls for a particular formed grade Compare demonstrated performance and service costs for equivalent grades

Specified this way, a fill order turns into an enforceable document. Which matters most when something goes wrong and the invoice for the failure lands on the bed.

When the Dew Point Slips: Failure Attribution and Bed Health

When outlet dew point rises, verify the measurement first. Check sensor condition, sampling flow and sampling pressure. A reading at a different pressure or before the sample line has stabilized can mislead the diagnosis.

Next, review inlet pressure, temperature and flow against the dryer rating. Inspect the separator, drains and upstream filters for carryover. Compare both towers over a complete cycle, watching valve operation, purge flow, exhaust restrictions, heating or cooling where applicable, and repressurization. Valve leakage can let wet air bypass the bed, while inadequate purge can leave residual moisture after regeneration. Once these checks point to the media, evaluate contamination, settlement and fines before approving a changeout. See the desiccant air dryer troubleshooting guide for a symptom-by-symptom sequence.

Oil aerosols and vapor can reduce the bed’s usable capacity if they reach the media. Check for abnormal compressor carryover and verify that upstream treatment addresses the form of oil present. A coalescing filter removes aerosols. Vapor removal, if required, calls for an appropriate separate treatment stage. Correct the source of contamination and follow the dryer manufacturer’s guidance on whether the affected fill can remain in service.

Do not order a replacement fill until regeneration settings, switching valves, upstream oil filtration, and inlet conditions have been ruled out. And after a changeout, re-verify the regeneration configuration: a new bed run on old settings will age exactly the same way.

Drain and filter faults can produce symptoms that resemble bed failure. A blocked or failed drain can allow liquid to carry over into the dryer, and a loaded filter can raise differential pressure. Check both against their maintenance and operating criteria when dew point or pressure drop changes.

A dew point trend across several complete switching cycles is more useful than a single reading. An earlier rise near the end of one tower’s drying interval may indicate breakthrough, but changes in inlet moisture, flow or regeneration can shift the curve too. Compare the two towers under similar conditions and correlate the trend with maintenance and process changes.

기술자가 흡착식 공기 건조기 설비의 스테인리스강 파이프 샘플링 포트에서 휴대용 측정기를 사용하여 압력 이슬점을 측정하고 있다
Trend over snapshot: a dew point reading taken at a sampling port while the towers run through a full cycle.

When the evidence points to the fill, confirm the replacement grade, layer sequence and loading quantities. After changeout, verify outlet PDP, pressure drop and repeatability across both towers.

What to Check Before Replacing a Dryer Fill

Compare the proposed fill against the dryer’s original media specification and operating envelope. Vessel dimensions, airflow distribution, valve operation and regeneration all affect what the fill can deliver. Record the grade and lot installed in each tower so later operating trends can be tied back to the changeout.

Use the purchase specification to agree on acceptance values and methods before ordering. After commissioning, document inlet conditions and outlet PDP across full cycles and retain a baseline pressure-drop reading. These measurements help distinguish media performance from changes in the air supply or dryer operation.

Jalon supplies activated alumina for air dryers 그리고 4A 분자체. Share the approved media specification, target dew point and regeneration method to compare candidate grades and request the relevant test conditions and batch documentation.

Desiccant specification review

Get a Fill Specification Built for Your Towers

Send your target pressure dew point, regeneration method, tower volume and dryer model so Jalon can advise on candidate media and documentation.

Request a Fill Specification

참고 문헌

  1. 미국 에너지부. 압축 공기 시스템 성능 개선: 산업용 참고서.
  2. 캐나다 천연자원부. 에너지 효율 참고 가이드: 압축 공기.
  3. 영국 에너지 기술 목록. 에너지 절약 제어 기능이 탑재된 흡착식 공기 건조기.
  4. 국제표준화기구. ISO 8573-1:2010 — 압축 공기: 오염 물질 및 순도 등급.
  5. 국제표준화기구. ISO 7183:2007 — 압축 공기 건조기: 사양 및 시험.

공유하기:

목차

더 많은 게시물

분자체 솔루션이 필요하신가요?

전해질 탈수에 사용되는 JALON JLOED 분자 체

본 서신은 리튬 이온 배터리용 전해질 생산을 위해 유기 용매를 건조하는 데 사용하기 위해, 뤄양 자론 마이크로-나노 신소재 유한공사(Luoyang Jalon Micro-nano New Materials Co., Ltd)의 ‘분자 체 JLOED 3.0-5.0 MM’ 제품을 평가했음을 알려드리기 위한 것입니다. 미국 캘리포니아주 치코(Chico)에 위치한 당사의 연구개발 및 생산 시설에서 ‘분자체 JLOED 3.0-5.0 MM’ 제품을 사용하여 처리한 유기 용매는 10ppm 미만의 극히 낮은 수분 함량을 보여 당사의 규격을 충족하였습니다. 이 분자체 제품은 당사의 품질 요건을 충족하였으며, 리튬 이온 배터리 산업에서 유기 용매를 건조하는 데 사용하기를 적극 권장합니다. 또한 해당 회사의 기술 지원에 깊이 감사드립니다.

나노테크 에너지

관련 상품
극저온 공기 분리 장치 프로젝트
Yuntianhua United Commerce Co., Ltd. 52,000 Nm³/저온 공기 분리 설비 프로젝트

뤄양 자론 마이크로-나노 신소재 유한공사의 JLPM 시리즈 분자체는 주로 일반 산업용 가스의 극저온 건조에 사용됩니다. 공기 분리 장치의 정제 시스템은 H₂O와 CO₂를 제거할 뿐만 아니라, 천연가스 및 기타 탄화수소의 탈황(H₂S 및 머캡탄 제거)과 CO₂ 제거도 수행합니다.

 

특히 언급할 만한 점은 Yuntianhua United Commerce Co., Ltd.의 52,000 Nm³/저온 공기 분리 장치 프로젝트입니다. 이 공기 분리 장치의 설계 및 제조 방식은 공기 및 흡착기에 수직 방사형 흐름 설계를 채택하였으며, 처리 용량은 311,352 Nm³/h입니다. 5.13 bar(A)의 흡착 압력, 당사의 JLPM3 고효율 분자 체 92톤과 활성 알루미나 107톤을 적재하여, 공기 중 이산화탄소(CO₂) 함량이 평균 1,000 ppm(2,000 PPM)인 상태에서도 장비의 즉각적이고 안정적인 작동을 보장하며, 분자 체에서 배출되는 CO₂는 0.1 PPM 미만입니다.

5세대 고성능 분자체 JLPM1은 공기 분리 설비의 예비 정제 장치(APPU)에 사용되는 첨단 분자체입니다. 이전 세대에 비해 5세대 고성능 분자체 JLPM1은 CO₂ 흡착 능력이 크게 향상되었으며, 공기 분리 설비 설계자 및 운영자에게 다양한 이점을 제공할 것입니다. 새로운 공기 분리 플랜트를 설계할 때, 5세대 고성능 분자체 JLPM1을 적용하면 공기 분리 설비의 설치 면적을 줄일 수 있어, 이에 따라 설비 투자 비용과 운영 비용을 절감할 수 있습니다. 또한, 5세대 고성능 분자체 JLPM1은 기존 설비의 개조에도 사용할 수 있어, 에너지 소비를 줄이거나 공기 분리 처리 능력을 향상시킬 수 있습니다.

관련 상품
주하이 웨위펑 철강 유한공사 30,000Nm³/h 압력 변동 흡착(VPSA) 방식 산소 생산 프로젝트

산소 분자체는 VPSA 산소 생산 장비의 원활한 작동을 보장하는 데 중요한 소재입니다. 이번 프로젝트는 당사의 JLOX-103 리튬계 고효율 산소 분자체의 또 다른 성공 사례입니다.

 

CSSC 황강 귀금속 유한공사가 설계 및 시공한 주하이 웨위펑 철강 유한공사의 30,000Nm3/h 압력 변동 흡착(VPSA) 산소 생산 프로젝트가 2019년 6월 27일 성공적으로 가동을 시작했습니다. 2020년 5월 29일 현재, 이 설비는 11개월 동안 안정적으로 가동되고 있으며, 모든 지표가 설계 지표를 상회하고 있습니다. 고객들로부터 높은 평가와 찬사를 받았으며, 기업에 연간 1억 5천만 위안의 누적 효과를 창출했습니다. 동시에, 이 프로젝트는 지능형 산소 생산, 모바일 제어 및 원격 모니터링을 통해 생산을 지도함으로써, 산업의 친환경적이고 지능적인 발전을 실현하는 데 기여하고 있습니다.

 

이 프로젝트는 4대의 압력 변동 흡착(VPSA) 방식 산소 발생기를 병렬로 사용합니다. 단일 장치 1대는 시간당 7,500Nm³의 산소를 생산하고, 산소 순도는 80%로 설계되었습니다. 이 장비에는 당사(뤄양 자론 마이크로 나노 신소재 유한공사)의 JLOX-103 리튬계 고효율 산소 분자체 68톤이 충전되어 있으며, 실제 산소 생산량은 7,650Nm³/h에 달하고 산소 농도는 82.3% 이상입니다. 이 프로젝트의 4세트 장비에는 당사의 JLOX-103 산소 분자체 272톤이 충전되어 있으며, 총 산소 생산량은 30,000Nm³/h를 초과합니다.

 

산소 분자체는 VPSA 산소 생산 설비의 가동을 보장하는 데 중요한 소재입니다. 이번 프로젝트는 당사의 JLOX-103 리튬형 고효율 산소 분자체의 또 다른 성공 사례입니다.

뤄양 자론 마이크로-나노 신소재 유한공사의 JLOX-100 시리즈 고효율 산소 발생 분자체는 리튬 X형 알루미노실리케이트 결정으로, 국제적으로 선진적인 수준의 산소 발생 분자체입니다. 철강, 비철금속, 화학 산업, 용광로 에너지 절약 개조, 환경 보호, 제지, 양식, 의료 등 다양한 산업 분야에서 널리 사용됩니다.

관련 상품